伦理午夜泡泡视频_一级片好爽黄色视频_日韩 欧美 综合_亚洲欧美日韩动图自偷自拍_婷婷综合激情五月在线_午夜成人性刺激免费视频_88国产精品欧美一区二区三区_99久久精品免费福利看国产_亚洲三级精品在线_人妻中文字幕系列在线看

ZJ-DR6200 series
Organic silicon thermal conductive gel

The two-component 1:1 mixed silicone thermal conductive gel is mainly used in communication, electronics, instruments, servers, automotive electronic parts, avionics, consumer electronics, high power microprocessors, power modules, etc.

Product features

It can be cured at room temperature or heated to form a low hardness elastic body that can be calendered, with the characteristic of faster curing at higher temperatures. During the curing reaction, there are no by-products, low shrinkage, no corrosion, no precipitation of low molecular weight silicone oil, automatic dispensing, and low installation stress. After solidification, the chemical properties are stable and there is no powdering phenomenon, which can reliably dissipate heat for power electronic devices.

Product parameters
Main parameters of ZJ-DR6200 series
Physical property items Unit Test method

ZJ-DR

6200-1

ZJ-DR

6200-2

ZJ-DR

6200-3

ZJ-DR

6200-4

ZJ-DR

6200-5

ZJ-DR

6200-6

Before curing

Viscosity(mpa.s)

A

GB/T 2794

10500

90000

110000

194800

200000

220000

B

GB/T 2794

26000

120000

130000

180000

220000

230000

Density(g/cm3)

A

GB/T 13354

1.8

2.1

3.0

3.3

3.4

3.4

B

GB/T 13354

1.8

2.1

3.0

3.3

3.4

3.4

Mixed density(g/cm3)

A+B

GB/T 13354

1.8

2.1

3.0

3.3

3.4

3.4

Operable time/23℃(h)

A+B

GB/T 7123

1

1

1

1

1

1

Gel time/23℃(h)

A+B

/

6

6

6

6

6

6

Curing conditions(℃×min)

A+B

/

120×30

120×30

120×30

120×30

120×30

120×30

After curing

Density/23℃(g/cm3)

GB/T 13354

1.8

2.05

3.0

3.3

3.4

3.4

shore(00)

/

45

45

50

50

55

65

Volume resistivity(Ω·cm)

GB/T 1692

1014

1013

1013

1011

1013

1013

Dielectric strength(KV/mm)

GB/T 1695

14

13

13

13

13

13

Flame retardancy

/

V0

V0

V0

V0

V0

V0

Thermal conductivity(W/ m.k)

TCI-2-A

1.0

2.0

3.0

4.0

5.0

6.0

Note: The above performance data were measured at 23 ± 2 ℃ and a relative humidity of 50 ± 5%. The data in the table is for reference only, please refer to the measured data.
Operation and Safety
  • Before use, components A and B should be thoroughly stirred separately, and then components A and B should be thoroughly mixed evenly in a 1:1 mass ratio. Stir for 5 minutes and apply glue within 40 minutes.
  • It is recommended that after applying the thermal conductive gel, it should be de foamed under the vacuum of -0.09MPa~-0.08MPa for 5-10 minutes, then it should be left to level for 20 minutes before being heated and cured.
  • Temperature and curing time: 23 ℃, after mixing A and B, the surface begins to dry at 2.0 hours; When the temperature is lower than 23 ℃, the gel time becomes longer; Above 23 ℃, with a surface drying time of less than 2.0 hours; Fully cure at 120 ℃ for 30 minutes.
  • The mixed adhesive should be sealed, stored, and used up within a safe operating period, otherwise it will slowly solidify and cause waste.
  • This product is not a hazardous material, but do not enter or eye contact. If accidentally splashed, rinse with plenty of water.
  • Do not contact with N, P, S, plasma compounds such as sulfur, polysulfide, polysulfone or other sulfur containing materials, amine, polyurethane, amide and azide, organotin compounds and silicone rubber containing organotin catalysts to avoid poisoning the platinum catalyst poisoning and curing failure.
Color and packaging

Pack a set of 20Kg components A and 20Kg components B (small barrels), or a set of 200Kg components A and 200Kg components B (large barrels).

Storage and expiration date

Store in a dry place for a storage period of 6 months (at 25 ℃). If it expires, it needs to be retested and can be used again after passing the inspection. This type of product belongs to non hazardous goods and can be transported as general chemicals. The A and B components of the colloid must be sealed and stored to prevent leakage during transportation!